The list shows typical densities of various paper grades.
| PAPER GRADES | POUND/CUBIC INCH (lb/in3) | GRAM/CUBIC CENTIMETER (g/cc) |
Tissue |
0.009 - 0.018 | 0.25 - 0.50 |
Wax Paper |
0.017 - 0.028 | 0.47 - 0.78 |
|
Uncoated Woodfree |
0.017 | 0.49 |
|
Tag Paper |
0.019 | 0.53 |
Unbleached Kraft |
0.021 - 0.025 | 0.58 - 0.69 |
Corrugated Medium |
0.022 | 0.61 |
News/Catalog/Directory |
0.022 - 0.025 | 0.61 - 0.69 |
CRS |
0.024 - 0.028 | 0.66 - 0.78 |
Pulp Sheet |
0.025 | 0.69 |
|
Book Paper |
0.026 | 0.72 |
|
Bond Paper |
0.027 | 0.75 |
Fine Paper |
0.028 | 0.78 |
Carbonizing Tissue |
0.028 | 0.78 |
Bleached Kraft |
0.030 | 0.83 |
Letterpress/ Offset |
0.031 | 0.86 |
|
Cover |
0.033 | 0.92 |
|
Index Paper |
0.034 | 0.94 |
Coated & Super Calendered Publication |
0.040 - 0.042 | 1.11 - 1.16 |
Super Calendered Glassine |
0.042 - 0.055 | 1.16- 1.52 |
HOME| PULP| PAPER| CONVERTER| DISTRIBUTORS| CONSULTANT| MACHINERY| CONTROL | CHEMICAL | SCHOOL | ORGANIZATION| MAGAZINE| ENGINEERING CAL.| |EMPLOYMENT| DICTIONARY/GLOSSARY| ACRONYMS/ABBREVIATIONS | PAPER GRADES | PULP GRADES | RESOURCES | WASTE MANAGEMENT| PAPERMAKING| TESTING| REPAIR | LISTING| ADVERTISEMENT | SITE MAP|