PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR SOUTH AMERICA
| S.N. |
Particular |
|
Time of Information |
Source |
| 01 |
Continent |
South America (North & South America
minus USA & Canada) |
|
|
| 02 |
Population (Million) |
650.0 |
2019 |
https://en.wikipedia.org |
| 03 |
Total Pulp/Paper/Paperboard Production |
22.3 |
2019 |
FAO |
| 03.1 |
Corrugated/Packaging |
13.48 |
| 03.2 |
Newsprint |
0.39 |
| 03.3 |
Graphic Paper (New Classification) |
4.03 |
| 03.4 |
Others |
4.20 |
| 04 |
Import |
9.36 |
| 05 |
Export |
3.38 |
| 06 |
Net Consumption |
28.3 |
| 07 |
Per Capita Consumption (Kg./year/person) |
44 |
| 08.0 |
Recovered Paper: Collection |
12.61 |
| 08.1 |
Import |
2.44 |
| 08.2 |
Export |
0.49 |
| 08.4 |
Consumption/Usage |
14.56 |
| 09.0 |
Wood
Pulp:
Production |
29.23 |
| 09.1 |
Import |
1.81 |
| 09.2 |
Export |
22.98 |
| 09.4 |
Consumption/Usage |
8.06 |
| 10 |
No. of Pulp/Paper Mills |
|
|
|
| 11 |
Main Raw Materials |
Wood |
|
|
| 12 |
Major Companies |
|
|
|
All Production, Import, Export and Net Consumption numbers are in Million
Metric Tons (1,000,000,000 Kg.)
Please provide if you have the latest info. If you want to write a Blog
please send me at wecare@paperonweb.com
and I will review it and publish