PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR CHINA

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country China    
02 Population (Million) 1376.05 2015 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 111.15 2015 FAO
03.1 Corrugated/Packaging 68.63
03.2 Newsprint 2.977
03.3 Writing & printing 25.639
03.4 Others 15.0
04 Import 4.497
05 Export 6.656
06 Net Consumption 108.991
07 Per Capita Consumption (Kg./year/person) 78.0
08.0 Recovered Paper: Collection 53.788
08.1                              Import 29.88
08.2                              Export 1.042
08.4                              Consumption/Usage 82.63
09.0 Wood Pulp:           Production 10.249
09.1                              Import 20.56
09.2                              Export 0.086
09.4                              Consumption/Usage 30.725
10 No. of Pulp/Paper Mills >500    
11 Main Raw Materials Recovered Paper, Wood, Bamboo & Market Pulp    
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)
Please provide if you have the latest info. If you want to write a Blog please send me at harigoyal@yahoo.com and I will review it and publish

Market Report on China’s Paper-making Industry, 2008-2010

Nov 21, 2008 – Summary
In 2007, China had 3500-4000 legal paper-making enterprises with a total production of 73.5 million tons, increased by 13.08% as compared with 65 million tons in 2006. Consumption reached 72.9 million tons, a 10.45% increment over the last year's 66 million tons, annual consumption was 55 kilograms per capita, increased by 5 kilograms.

Production increased by 140.98% from 2000 to 2007, and consumption 103.92%. Production and consumption of paper and cardboard increased by 13.39% and 10.72% respectively, 2000-2007, surpassing China's GDP annual growth rate of the same period.
According to the production and consumption of 2007, both kept continuous growth all the year round, however, growth rate of production weakened. A larger increase of production can be seen in those products such as newsprint, coated paper, household paper, coated white board, boxboard and corrugated paper. And newsprint, copperplate paper, boxboard as well as corrugated paper have a larger increase in consumption.

Click here for complete news release

Top 5 Non-Wood Pulp Producing Countries (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 12.3 0.55 0.52 12.4
China 6.8 0.04 0.08 6.8
India 2.0 0.0 0.0 2.0
Spain 0.83 0.0 0.02 0.82
Pakistan 0.37 0.0 0.0 0.37
USA 0.32 0.02 0.08 0.26

Top 5 Paper & Paperboard Producing Countries  (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 406.3 105.5 110.6 401.2
China 111.1 4.5 6.6 109.0
USA 72.4 9.5 11.6 70.3
Japan 26.2 1.8 1.5 26.5
Germany 22.6 10.7 13.2 20.0
India 15.0 2.3 0.57 16.7

Top 5 Recovered Paper Producing/Collection Countries  (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 225.1 57.4 56.9 225.5
China 53.8 29.9 1.04 82.6
USA 47.8 0.76 19.6 28.4
Japan 21.8 0.04 4.3 17.5
Germany 15.2 4.0 2.5 16.7
Korea Republic (South) 8.3 1.54 0.55 9.3

Top 5 Wood Pulp Importing Countries  (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 175.6 58.7 59.1 175.3
China 10.2 20.6 0.08 30.7
USA 49.4 5.4 7.7 47.0
Germany 2.6 4.8 1.2 6.2
Italy 0.41 3.5 0.05 3.8
Korea Republic 0.40 2.3 0.00 2.7

Top 5 Non-Wood Pulp Importing Countries (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 12.3 0.55 0.52 12.4
Saudi Arabia 0.0 0.11 0 0.11
Germany 0 0.08 0.04 0.041
China 6.8 0.041 0.08 6.76
Japan 0 0.031 0.0 0.036
UK 0 0.03 0.0 0.032

Top 5 Recovered Paper  Importing Countries  (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 225.1 57.4 57.0 225.5
China 53.8 29.9 1.04 82.6
Germany 15.2 4.0 2.54 16.7
India 2.64 3.08 0 5.72
Netherland 2.2 2.32 2.6 1.96
Indonesia 3.9 1.7 0.02 5.61

Top 5 Non-Wood Pulp Exporting Countries (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 12.3 0.55 0.52 12.3
USA 0.32 0023 0.084 0.26
China 6.8 0.041 0.082 6.8
Thailand 0.116 0.010 0.044 0.082
France 0.08 0.03 0.042 0.066
Germany 0.0 0.08 0.038 0.041

Top 5 Wood Pulp Consuming Countries (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 175.6 58.7 59.07 175.3
USA 49.4 5.35 7.73 47.0
China 10.3 20.6 0.09 30.7
Japan 8.87 1.68 0.44 10.14
Sweden 11.6 0.39 3.48 8.5
Canada 17.6 0.33 917 8..0

Top 5 Non-Wood Pulp Consuming Countries (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 12.34 0.54 0.52 12.37
China 6.8 0.04 0.082 6.76
India 2.0 0.0 0.0 2.0
Spain 0.83 0.0 0.0 0.82
Pakistan 0.37 0.0 0.0 0.37
USA 0.32 0.023 0.084 0.26

Top 5 Paper & Paperboard Consuming Countries  (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 406.3 105.5 110.6 401.2
China 111.1 4.5 6.6 109.0
USA 72.4 9.5 11.6 70.3
Japan 26.2 1.8 1.5 26.5
Germany 22.6 10.7 13.2 20.1
India 14.96 2.3 0.57 16.72

Top 5 Recovered Paper Consuming Countries  (Million Metric Ton in 2015)

Countries Million MT
  Production Imports Exports Net Consumption
World 225.1 57.4 56.97 225.5
China 53.8 29.9 1.04 82.6
USA 47.3 0.71 19.6 28.5
Japan 21.8 0.035 4.3 17.5
Germany 15.2 3.99 2.54 16.7
Korea (South) 8.33 1.54 0.55 9.3