PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR AUSTRIA
| HOME | COUNTRY WISE STATISTICS |
| S.N. | Particular | Time of Information | Source | |
| 01 | Country | Austria | ||
| 02 | Population (Million) | 8.9 | 2020(E) | http://en.wikipedia.org |
| 03 | Total Pulp/Paper/Paperboard Production | 4.985 | 2019 | FAO |
| 03.1 | Corrugated/Packaging | 2.395 | ||
| 03.2 | Newsprint | 0.290 | ||
| 03.3 | Graphic Paper (New Classification) | 2.280 | ||
| 03.4 | Others | 0 | ||
| 04 | Import | 1.286 | ||
| 05 | Export | 4.166 | ||
| 06 | Net Consumption | 2.105 | ||
| 07 | Per Capita Consumption (Kg./year/person) | 235 | ||
| 08.0 | Recovered Paper: Collection | 1.399 | ||
| 08.1 | Import | 1.491 | ||
| 08.2 | Export | 0.312 | ||
| 08.4 | Consumption/Usage | 2.578 | ||
| 09.0 | Wood Pulp: Production | 2.090 | ||
| 09.1 | Import | 0.628 | ||
| 09.2 | Export | 0.450 | ||
| 09.4 | Consumption/Usage | 2.269 | ||
| 10 | No. of Pulp/Paper Mills | Wood | ||
| 11 | Main Raw Materials | |||
| 12 | Major Companies |
All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.) Please provide if you have the latest info. If you want to write a Blog please send me at wecare@paperonweb.com and I will review it and publish
Austrian Paper Industry - Key Data 2015
Companies............24 Production.............4.96 Million MT