Q.1095: What is difference between cardboard and corrugated board?
Ans. Cardboard is a stiff and thick single or multi-ply paperboards. Cardboards are typically made from bleached pulp and use recycled fiber.
Corrugated board is a pasted single or double-faced multilayered type of board in which the bottom or middle layer is fluted. Flute is made from unbleached pulp. Liners are also mostly made from unbleached pulp. Various types of corrugated boards.

Open Face Single Face Single Wall

Double Wall Triple Wall