Q.1088: What is C6 sheet size? , What is iso c6?
Ans. The C series is used for folders, post cards and envelopes. C series envelope is suitable to insert A series sizes.
As per ISO (International Standard Organization) C series cut sheet sizes, C6 is 114 mm wide and 162 mm long sheet. Equivalent size in inches is 4.51" wide and 6.38" long.
For all ISO and US sizes, click here