Q.1082: What is C0 sheet size? , What is iso c0?
Ans. The C series is used for folders, post cards and envelopes. C series envelope is suitable to insert A series sizes.
As per ISO (International Standard Organization) C series cut sheet sizes, C0 is 917 mm wide and 1297 mm long sheet. Equivalent size in inches is 36.10" wide and 51.06" long.