Q.1013: Can paper be made from grass?
Ans. Yes. Bamboo is a part of grass family and used for making paper in most of east and south east Asia. In fact it is main raw material for making paper in India. Other grass used for making paper are esparto, elephant grass etc.

Bamboo Esparto Elephant Grass
However your lawn grass or other short grasses can't be used to make paper.