Q.1050: Can we make paper from algae or seaweeds?
Ans. NO.
Although they have many plant-like features seaweeds are not true vascular plants; they are algae. Algae are part of the Kingdom Protista, which means that they are neither plants nor animals. Seaweed are not made of cellulose fibers, hence not suitable to make paper.