Q.1029: What is the density of paper
Ans. Density of paper varies from 0.25 (soft tissue) to 1.5 (super calendered glassine) gm/cm3. Just for comparison density of water is 1.0 gm/cm3.
In English unit, density of paper varies from 15.5 (soft tissue) to 93 (super calendered glassine) lbs/ft3. Just for comparison density of water is 62.4 lbs/ft3.
To see the density of other paper visit www.paperonweb.com/density.htm